ISO 11357 High Temperature Differential Scanning Calorimeter

ISO 11357 High Temperature Differential Scanning Calorimeter

ISO 11357 High Temperature Differential Scanning Calorimeter

Understanding ISO 11357

ISO 11357 is a fundamental international standard fordifferential scanning calorimetry (DSC) of plastics, polymers, and other thermally stable materials. It specifies the principles, apparatus, calibration, and test procedures for measuring key thermal properties such as glass transition temperature (Tg), melting temperature (Tm), crystallization temperature (Tc), enthalpy of fusion, crystallization enthalpy, oxidation induction time (OIT), and oxidation induction temperature.

Compliance with ISO 11357 ensures test results are accurate, repeatable, and internationally comparable, making it essential for material R&D, quality control, production inspection, and certification in polymer, chemical, automotive, electronics, and aerospace industries.

 

Working Principle of Differential Scanning Calorimeter

DSC technology measures the change in temperature difference (heat flow) between a sample and a reference as a function of time or temperature. The sample and reference are placed in a homogeneous temperature zone.

 

When the sample exhibits no thermal transition, temperatures at both the sample and reference sides follow the programmed temperature profile. When the sample undergoes a physical or chemical change such as melting, crystallization, or decomposition, heat is absorbed or released to drive the transition. As a result, the reference temperature continues to rise with the furnace, while the sample temperature deviates, creating a measurable temperature difference. This temperature difference is recorded as a curve, forming the original DSC data for thermal analysis.

 

Applications

This automatic digital DSC testing machine is widely used in:

– Plastic, rubber, fiber, and composite material R&D

– Chemical industry and new material development

– Automotive and electronic component reliability testing

– Quality inspection and production quality control

– Universities, research institutes, and third‑party testing laboratories

 

It is widely applied to characterize melting, crystallization, glass transition, curing, crosslinking, thermal stability, oxidation induction, and phase transitions, providing critical data for material selection, process optimization, and quality assurance.

 

Applications and Value

This automatic digital DSC testing machine is widely used in aerospace, electronics, automotive, chemical, packaging, and university research fields, as well as third-party testing laboratories. Its core applications include thermal property characterization of plastics, rubbers, fibers, composites, and new materials—covering melting, crystallization, glass transition, curing, and oxidation induction—providing critical data for material R&D, process optimization, and quality control.

By adhering to ISO 11357, the High-Temperature Differential Scanning Calorimeter ensures standardized, globally consistent thermal analysis results. Its high precision, stability, and intelligent automation make it a reliable solution for enterprises and research institutions to meet quality assurance and international market access requirements.