Coating defects and treatment methods
Coating defects and treatment methods Spray coating technology often has various defects in the coating process, the causes of these defects and the corresponding treatment methods are as follows: Bublina: Cause The paint viscosity is too high. The filter of the coating machine failed. Paint conveying pressure is too high. The paint circulates in the device for too long, resulting in increased viscosity and bubbles. The distance between the knife edge of the spray head and the surface to be coated is too large, resulting in increased...